posted on 1999-09-02, 00:00 authored by Maria ForsythMaria Forsyth, S Wong, K Nairn, A Best, P Newman, D MacFarlane
27Al, 31P and 7Li NMR measurements have been performed on lithium conducting ceramics based on the LiTi2(PO4)3 structure with Al, V and Nb metal ions substituted for either Ti or P within the framework NASICON structure. The 27Al magic angle spinning NMR measurements have revealed that, although Al is intended to substitute for octahedral Ti sites, additional substitution into tetrahedral environments (presumably phosphorous sites) occurs with increasing amount of Al addition. This tetrahedral substitution appears to occur more readily in the presence of vanadium, in Li1+xAlxTi2−x(PO4)2.9(VO4)0.1, whereas similar niobium additions (in place of vanadium) appear to stifle tetrahedral substitution. 7Li static NMR spectra reveal quadrupolar structure with Cq approximately 42 kHz, largely independent of substitution. Measurement of the 7Li central transition linewidth at room temperature reveals a relatively mobile lithium species (300–900 Hz) with linewidth tending to decrease with Al substitution and increase with increasing V or Nb. This new structural information is discussed in the context of ionic conduction in these ceramics.

History

Journal

Solid state ionics

Volume

124

Issue

3-4

Pagination

213 - 219

Publisher

Elsevier

Location

Amsterdam, The Netherlands

ISSN

0167-2738

eISSN

1872-7689

Language

eng

Publication classification

C1.1 Refereed article in a scholarly journal

Copyright notice

1999, Elsevier Science B.V.